3D printing settings glossary (slicing software, or slicer). Written for Canada, in Canadian English. A price in Canadian dollars is shown only when this site has already checked a Canadian shop; euro amounts from the English edition are not converted and are not repeated here. Shop links open .
Reference · settings
3D printing settings glossary (slicing software, or slicer) — Canada
When you open the software that prepares your prints for the first time, you face dozens of settings with mysterious names. This glossary explains them one by one, in plain words: what each setting does, which value to start with, and what happens if you raise or lower it.
Step 4 of 6 · Updated 30 October 2026 · Data: official manufacturer spec sheets
Print faults in pictures
Many of the settings below exist to avoid one specific fault. Here is what the most common ones look like, so you can recognise them on your own parts. Each is covered, with the checks to make, in the common beginner problems.

Lifting corners (“warping”)
The edges or corners of the part peel off the bed and curl up, sometimes until the part comes off completely. The cause: the plastic shrinks a little as it cools and pulls on the edges. The larger the base, the stronger the pull. The diagram shows the simplest remedies.

Stray threads between parts (“stringing”)
Fine threads of plastic, like spider webs, stay stuck between two parts of the object or around it. The nozzle let a little plastic ooze while it was moving without printing. The usual causes: a nozzle that is too hot, a filament pull-back (the retraction) that is too small, or damp plastic.

Failed first layer
The lines of the first layer stick neither to each other nor to the bed, are too thin or too squashed, or the part “rolls” under the nozzle. Almost always, the nozzle is too high or too low (see the diagram), or the bed is dirty or not level.

A first layer that is too squashed, or a bed that is too hot, also causes another fault: the base of the part flares out slightly, like an elephant’s foot.

Not enough plastic (“under-extrusion”)
The nozzle lays down less plastic than planned. You see small holes in the walls, incomplete layers, lines that do not touch each other, sometimes a regular “click-click” from the extruder, the mechanism that pushes the thread. Usual causes: a partly clogged or too-cold nozzle, too high a speed, damp plastic.
There is no free-licence photo to show you for this fault yet: spot it from the description above, then confirm with the visual symptom diagnostic tool.
Too much plastic (“over-extrusion”)
Conversely, the nozzle lays down more plastic than planned: surfaces look bulging or bumpy, corners are rounded and the part is slightly larger than the model, which stops two parts from fitting together. Usual causes: a flow setting that is too high or a line width that is too large.
There is no free-licence photo to show you for this fault yet: spot it from the description above, then confirm with the visual symptom diagnostic tool.
Shifted layers
From a certain height, the upper part of the part is shifted sideways, as if the upper storey of a house had been slid across. The print head lost its position while working. Usual causes: a belt (the toothed band that drives the head) that is too loose, a head that hit the part, a speed or acceleration that is too high.

Small balls of plastic (“blobs”)
Small balls or smears of plastic appear on the surface, often where each outline starts and ends (the seam) or in corners. They come from plastic pressure in the nozzle that is badly compensated, or from a poorly set filament pull-back.
There is no free-licence photo to show you for this fault yet: spot it from the description above, then confirm with the visual symptom diagnostic tool.
Vibration echoes (“ghosting”)
Around a corner, a hole or a raised letter, you see faint ripples that repeat the outline, like an echo or a shadow. It is called “ghosting” or “ringing”. They come from the machine vibrating after a sudden change of direction: speed or acceleration too high, a slack belt, a wobbling table.
There is no free-licence photo to show you for this fault yet: spot it from the description above, then confirm with the visual symptom diagnostic tool.
Overhanging parts that sag
When the plastic stays too hot, the parts that stick out into the void (the overhangs) sag or deform. The fan on the print head is there to set them quickly.

The settings, one by one
Click a setting in the index, or scroll through the list. To put these values into practice, go through the first printer setup.
Acceleration
Definition. How quickly the nozzle goes from standstill to its cruising speed, at the start or at every change of direction. It is measured in mm/s²: with 1,000 mm/s², the speed rises by 1,000 mm/s every second, so the nozzle reaches 50 mm/s in a twentieth of a second.
| Typical values | Too low | Too high |
|---|---|---|
| Between 1,000 and 5,000 mm/s² for a beginner. The setting proposed by the machine’s maker is the best starting point. | The print is a little longer, but there are fewer visible vibrations on the part. | The jolts make the machine vibrate: you see echoes of faint ripples repeating the outline of corners or letters (“ringing”, or “ghosting”). If it is too violent, a motor can even miss steps and shift the layers. |
Bed temperature
Definition. The temperature of the heated surface the part is built on. A warm bed helps the first layer stay stuck.
| Typical values | Too low | Too high |
|---|---|---|
| For PLA, between 55 and 65 °C; 60 °C to start. | The part sticks poorly: corners lift (this is “warping”) or the part comes off during printing. | The first layers soften and squash: the base of the part flares out slightly, like an elephant’s foot. |
Brim and raft
Definition. The brim is a flat border printed around the base of the part, like the brim of a hat, to stick it better to the bed. The raft is a small floor printed under the whole part, which serves as a sacrificial base.
| Typical values | Too low | Too high |
|---|---|---|
| A 5 to 8 mm brim if the part struggles to stay stuck; the raft is rarely useful for a first PLA. | Without a brim, a part with a large base risks having its corners lift (“warping”). | With a raft, the underside of the part turns rough, and you lose time and plastic. |
Flow (extrusion multiplier)
Definition. A factor that adjusts the amount of plastic pushed towards the nozzle. At 1.00, the machine pushes exactly the calculated amount; at 0.95, a little less.
| Typical values | Too low | Too high |
|---|---|---|
| 1.00 to start; between 0.95 and 1.05 once tuned. | Not enough plastic: small gaps between lines and walls that are too thin (under-extrusion). | Too much plastic: bulging surfaces and dimensions slightly too large (over-extrusion). |
Infill (density)
Definition. The amount of plastic placed inside the part, as a percentage: 0% for a hollow part, 100% for a solid one. This structure is hidden beneath the walls.
| Typical values | Too low | Too high |
|---|---|---|
| Between 15 and 25% for a decorative object; more for a part under load. | The part is fragile, and the top can sag or dip for lack of support underneath. | Much more time and plastic for very little extra strength. |
Infill patterns
Definition. The shape of the pattern inside the part: grid, continuous waves (“gyroid”), cubes… Like corrugated cardboard, it spreads the load.
| Typical values | Too low | Too high |
|---|---|---|
| A grid or a gyroid are good compromises to start with. | A pattern that is too open under a thin top: the top sags or lets the structure underneath show through. | A very dense pattern amounts to raising the infill percentage: it is better then to raise that percentage rather than change pattern. |
Layer height
Definition. The thickness of each layer of plastic laid down. Think of slices of bread: the thinner they are, the smoother the surface, but the more of them you need.
| Typical values | Too low | Too high |
|---|---|---|
| Between 0.16 and 0.20 mm with a 0.4 mm nozzle: a good balance between fineness and time. For scale, 0.2 mm is roughly the thickness of two sheets of paper. | A finer surface and sharper detail, but the print becomes very long. If you go too low, the nozzle may struggle to push enough plastic and holes appear in the walls. | A faster print, but you see small steps on curved or sloping surfaces, like staircases. As a rule, do not go above 75% of the nozzle diameter (0.3 mm for a 0.4 mm nozzle), otherwise the layers bond less well to each other. |
Line width
Definition. The width of the bead of plastic the nozzle lays down. It is usually close to the nozzle diameter.
| Typical values | Too low | Too high |
|---|---|---|
| Between 0.40 and 0.45 mm for a 0.4 mm nozzle. | Small gaps appear between the lines and the layers bond poorly: the part breaks more easily. | Too much plastic in the same space: bulging surfaces and a part slightly larger than planned (this is over-extrusion), which is a nuisance when two parts have to fit together. |
Nozzle temperature
Definition. The temperature at which the nozzle heats the plastic to melt it.
| Typical values | Too low | Too high |
|---|---|---|
| For PLA, between 210 and 220 °C; 215 °C is a good starting point. Always follow the label on your spool. | The plastic is too thick to come out steadily: poorly bonded layers, holey walls (this is under-extrusion, too little plastic), even a clogged nozzle. | The plastic becomes too runny: it drips from the nozzle, leaves fine threads between parts of the object (“stringing”) and the surface turns very shiny, even browned. |
Part cooling fan
Definition. The fan on the print head, which blows on the plastic just after it is laid down to cool and set it.
| Typical values | Too low | Too high |
|---|---|---|
| For PLA, often 100% from the 2nd or 3rd layer, keeping it off or low on the first so that it sticks. For ABS or ASA (plastics more heat-resistant than PLA): low or off. | With PLA, the parts that stick out into the void sag and small details melt. | With ABS or ASA, too much cooling makes corners lift (“warping”) and layers separate, which is called delamination. |
Pressure compensation (pressure advance, or linear advance)
Definition. The molten plastic is slightly compressed in the nozzle, like toothpaste in a tube: it keeps coming out for a moment when the nozzle slows down, and is slow to come out when it speeds up. This setting anticipates that lag.
| Typical values | Too low | Too high |
|---|---|---|
| Keep the value proposed by the machine’s maker; only adjust it once the first layer works well. | Small balls of plastic (“blobs”) or swollen corners, especially as the nozzle approaches corners. | Corners look “eaten away”: plastic is missing just after an acceleration, and lines start thin. |
Print speed
Definition. The speed at which the nozzle moves while laying down plastic, in millimetres per second (mm/s). At 50 mm/s, the nozzle advances 5 cm every second. Moves without printing have their own, higher speed.
| Typical values | Too low | Too high |
|---|---|---|
| Between 40 and 80 mm/s for a first PLA. The makers’ “fast” settings go much higher, but only on machines built for it. | The print takes longer, with no visible gain in quality. | The nozzle can no longer melt enough plastic in time: holey walls (under-extrusion) and vibrations that leave faint ripples around corners (“ringing”). |
Retraction (filament pull-back)
Definition. A small pull-back of the thread just before the nozzle moves without printing, so that the plastic does not ooze during the trip.
| Typical values | Too low | Too high |
|---|---|---|
| With an extruder mounted on the print head (“direct drive”), a pull-back of 0.5 to 1.5 mm is enough. With a remote extruder linked by a tube (“Bowden”), the pull-back is longer: follow the maker’s setting. | Fine threads of plastic stay stretched between two parts of the object (“stringing”). | Plastic is missing at the start of lines after each move, leaving small gaps; over time, the gear that pushes the thread wears out. |
Seam
Definition. The spot where each outline starts and ends. You sometimes see a small vertical line or slight bumps there.
| Typical values | Too low | Too high |
|---|---|---|
| “Aligned” or “rear” to hide it; “random” spreads the starting points over the whole part. | If badly placed, the seam is clearly visible on the front of the part. | In random mode, the surface looks slightly uneven everywhere, which can bother more than a single line. |
Supports
Definition. Temporary structures printed under the parts that stick out into the void (the overhangs), so that the plastic has something to rest on. They are broken off afterwards.
| Typical values | Too low | Too high |
|---|---|---|
| Turn them on when a part leans out by about 45 to 50 degrees from the vertical: beyond that, the plastic has almost nothing under it. | Without supports where they are needed, the plastic sags or falls in tangled threads (the part is said to turn into “spaghetti”). | Scarred surfaces where the supports were attached, tedious removal and wasted plastic. |
Top and bottom layers
Definition. The number of solid layers that close the top and bottom of the part, on either side of the infill.
| Typical values | Too low | Too high |
|---|---|---|
| 4 or 5 layers with a layer height of 0.2 mm, about 1 mm, for a properly opaque top. | The infill pattern shows through the top, which looks dented like a pillow (“pillowing”), and the surface is porous. | More time and plastic, with no visible difference. |
Top-surface ironing
Definition. After printing the top, the nozzle passes over it again with very little plastic, like an iron over fabric, to get a smoother surface.
| Typical values | Too low | Too high |
|---|---|---|
| Off for beginners; turn it on for a neat top if you accept a longer print. | Without ironing, the top keeps a visible grain, often perfectly acceptable. | The print takes longer, and if badly set, ironing risks overheating the surface locally. |
Walls (perimeters)
Definition. The number of outlines printed around the part, before the infill. These are the outer walls: they provide most of the strength.
| Typical values | Too low | Too high |
|---|---|---|
| 2 or 3 walls, i.e. 0.8 to 1.2 mm thick with a 0.4 mm nozzle. | The walls are thin and fragile; they may let liquid through if you want a watertight part. | The print takes longer and uses more plastic, for a strength gain that is mostly noticeable when you bend the part. |
Frequently asked questions
Where do these values come from?
They are common starting values, taken from the settings proposed by slicing programs (Orca Slicer, Cura, Bambu Studio) and from plastic makers’ data sheets. They are a starting point, not a final setting. See our method.
Where should I start in practice?
Go through the first setup first, then look up your PLA in the filament table, and come back here to understand one setting at a time.
How do I save my settings in Orca Slicer?
With the settings generator for Orca Slicer, which creates a file to load into the software and customise afterwards.
Sources
Sources checked on 30 October 2026. Printer prices shown are from official European stores in late October 2026 and may change. Technical figures come from manufacturer sheets and our calculations.
Written by Emmanuel Sauvage · Scan3D Lab
A question about this machine or guide? Ask it here
We read every message and reply by email, usually within a few days.