Which defect does the part show?. Written for the United Kingdom, in British English. A price in pounds is shown only when this site has already checked a UK shop; euro amounts from the English edition are not converted and are not repeated here. Shop links open .
Tool · FDM tuning
Which defect does the part show? — United Kingdom
Pick the symptom that looks most like your print. You get a likely cause, a first check you can do yourself, and the settings to find in OrcaSlicer, Bambu Studio and UltiMaker Cura.
Updated 24 October 2026
Routine care (user-replaceable): nozzles, PEI sheets, FEP/PFA film, PTFE tubes and cleaning per the manual. Manufacturer service recommended for mainboard, power supply, motors or heater faults under warranty (Bambu Lab, Creality, Elegoo, Anycubic, Sovol, 3DMakerpro).
Stringing (angel hair)
Fine threads between walls, mostly on travel moves or across hollow areas.
Difficulty2/5Time15–30 minCostthe price on Amazon.co.ukToolsFlush cutters, a gentle flame or a hairdryer (PLA only)
Likely cause:Nozzle too hot, retraction too short, or damp filament (typical of PETG).
What to try:Drop the nozzle temperature in 5 °C steps, lengthen and speed up retraction, and dry PETG or nylon for 4 hours at 50 °C.
Where to change it in the slicer
Setting
OrcaSlicer
Bambu Studio
Cura
Retraction
Filament → retraction length 0.8–1.2 mm (direct drive) or 4–6 mm (Bowden)
Filament → retraction length (PLA profile about 0.8 mm)
Travel → Retraction distance
Retraction speed
30–45 mm/s
Leave the filament profile value
Retraction speed 40 mm/s
Nozzle temperature
5 to 10 °C under the manufacturer profile
Filament → Nozzle temperature
Material → Printing temperature
Wipe
Enable “Wipe while retracting”
Advanced filament settings
Travel → Combing mode “Not in skin”
If you are unsure, if your machine is under warranty, or if the error persists after basic checks, contact official support or have the manufacturer repair your device.