Skip to content

Troubleshooting · beginner

Common beginner problems in filament (FDM) 3D printing

Your first part doesn’t look like what you expected: corners lifting, fine threads of plastic between the parts, plastic missing in places. These faults are very common with the first spools of PLA (the easiest plastic to print), and almost always easy to fix. By the end of this page you’ll be able to recognise each one, guess its most likely cause and know what to check first.

Step 6 of 6 · Updated 30 October 2026 · Data: official manufacturer spec sheets

On this page (6)
Golden rule. Change one thing at a time, then run a small test print: if you change five settings at once, you won’t know which one fixed (or worsened) the problem. For PLA, the usual starting point is a nozzle (the heated tip that melts the filament) at 215 °C and a bed (the surface the part is built on) at 60 °C; the temperature table by filament covers the other plastics. For rarer faults, see the symptom diagnostic and the error codes.

Corners that lift (“warping”)

What you see

The edges or corners of the part come away from the bed and curl upwards; sometimes the whole print comes loose midway. Plastic shrinks as it cools, like a cookie curling up: if the base isn’t stuck firmly enough to the bed, it lifts.

Diagram of an orange bed with four identical blue parts placed in four different ways to make them stick better.
Four ways to help a part stay stuck: a bed surface suited to the plastic, glue or adhesive tape, a flat border printed around the base (the “brim”) or a small floor printed underneath (the “raft”). We have no free photo of a lifted corner, so this diagram shows the remedies.Diagram: paulo@kiefe.com (STEMFIE.org), CC BY-SA 4.0 licence, via Wikimedia Commons — https://commons.wikimedia.org/wiki/File:3D_printing_calibration_3D_printer_build_plate_adhesion.png

Why it happens

  • The bed is too cold, or the first layer is too high and sticks poorly (see “The failed first layer” below).
  • The bed surface is dirty (fingerprints, dust) or poorly suited to the plastic used.
  • A cold draught hits a large part, or you are printing ABS (a plastic more sensitive to heat than PLA) without a closed enclosure around the printer.

What to check, in order

  1. Clean the bed as the manufacturer describes, then redo the levelling, meaning the adjustment of the distance between nozzle and bed (first setup).
  2. Check in the slicer (the program that prepares the file for the printer) that the bed is set to 60 °C for PLA; the spool label confirms the recommended range.
  3. Add a brim, the flat border printed around the base that enlarges the contact surface with the bed (brim in the glossary).

Stray threads between parts (“stringing”)

What you see

Fine threads of plastic, like spider webs, stay stuck between two areas of the part or around it, especially where the nozzle moved without printing.

Two blue 3D-printed figurines on a table, with fine white threads sticking out from the top of the head and the back.
Two blue figurines whose heads and backs carry fine white threads. These threads can be removed with a craft knife, but they signal a setting to correct. According to the photo’s author, they come from a flexible PLA printed too fast.Photo: j bizzie (Minneapolis, USA), CC BY 2.0 licence, via Wikimedia Commons — https://commons.wikimedia.org/wiki/File:Squirtle_army!_Frist_test_with_flexible_PLA,_do_need_to_drop_print_speed_down_as_suggested_by_-matterhackers_to_avoid_mohawk_wisps_(by_j_bizzie)_2014-12-09.jpg

Why it happens

  • The nozzle is too hot for this plastic: it becomes very runny and drips by itself.
  • The retraction is too small or too slow. This is the small pull-back of the filament that the printer makes before moving without printing, so that it doesn’t drip. The right setting depends on the extruder: direct drive (the motor that pushes the filament sits right on the nozzle) or Bowden (the motor is far away and the filament runs through a tube).
  • The plastic is damp, especially PETG, but also PLA left open for a long time: the water it contains turns to steam in the nozzle and makes the plastic ooze.

What to check, in order

  1. If the nozzle is set above the range printed on the spool label, lower it by 5 °C.
  2. Go back to the profile the manufacturer provides for your printer before raising the retraction blindly (retraction in the glossary).
  3. Dry the spool following the manufacturer’s procedure or with a filament dryer, then store it in a closed box.

The failed first layer

What you see

The lines of plastic stick neither to each other nor to the bed, they are too thin or too squashed, or the part “rolls” under the nozzle. This is the most important fault to fix, because every following layer rests on this one.

Diagram of the distance between nozzle and bed: on the left the right distance, on the right two wrong cases, nozzle too close and nozzle too high.
On the left, the right distance (green tick): the line is slightly flattened and well stuck. Top right, the nozzle is too close to the bed: the line is very thin. Bottom right, the nozzle is too high: the line hangs in the air and does not stick.Diagram: Stemfie3D (STEMFIE.org), CC BY-SA 4.0 licence, via Wikimedia Commons — https://commons.wikimedia.org/wiki/File:3D_printing_calibration_build_plate_first_layer_gap.png

Why it happens

  • The Z offset, meaning the gap set between the nozzle and the bed for the first layer, is wrong: the nozzle is too high or too low.
  • The flow, the amount of plastic the printer pushes out, is too low for the first layer: the line lacks the material to squash and stick.
  • The bed hasn’t been heated long enough before the start: the displayed temperature is reached, but the whole surface isn’t evenly hot yet.

What to check, in order

  1. Run the levelling or setup wizard of your printer again, then look at the line the printer draws at the start of the print (the purge line): it should be even and slightly flattened.
  2. Let the bed reach its temperature, then wait a few tens of seconds more before starting the print.
  3. Compare with the definitions of layer height and line width in the glossary.

Missing plastic (“under-extrusion”)

What you see

Holes appear in the walls, some layers are incomplete, the width of the plastic line varies, and you sometimes hear a small regular “click” from the extruder (the mechanism that pushes the filament): it slips because the filament isn’t moving. The printer isn’t laying down enough plastic, hence the name under-extrusion. A description and landmarks are also in the glossary of faults.

Why it happens

  • The nozzle is partly clogged, or too cold for the amount of plastic requested: the plastic doesn’t have time to melt.
  • The speed or acceleration (how quickly the head changes speed) are too high for what the hotend can melt. The hotend is the heated head that holds the nozzle.
  • The filament diameter or flow are set wrongly in the slicer: the program thinks it pushes more plastic than actually comes out.

What to check, in order

  1. Extrude by hand with the nozzle heated, following the manufacturer’s manual: the filament should come out as a continuous, even strand. If it comes out in jerks or not at all, the nozzle is probably clogged.
  2. Go back to a beginner speed (see speed in the glossary) before touching the flow.
  3. If the screen displays an error message (HMS codes on Bambu Lab, for example), look it up in the Bambu Lab, Creality, Elegoo and Anycubic error codes.

Going further

The visual symptom diagnostic also covers other faults, such as layer shift, when part of the object is shifted sideways. To understand each setting mentioned here, open the settings glossary; for the temperatures of each plastic, the temperature table by filament.

Takeaway. Look at what you see, spot the most likely cause, make one check, then a small test print. One change at a time, and don’t replace the machine before going through these steps.
Good to know. Lifting corners often come from a cold bed or a first layer that is too high. Stray threads often come from a retraction that is too small or from damp plastic. In both cases the plastic behaves like a cookie that curls up or a liquid that runs: these are effects of heat, not a machine breakdown.
Our take : look, spot the likely cause, make one check, then a small test. Don’t replace the machine before these steps; if you feel lost, the getting-started guide puts you back on track.

Frequently asked questions

Is the visual diagnostic translated?

The detailed tool is on the French-language site: visual symptom diagnostic. The page you are reading is translated.

Where do I look up a Bambu Lab HMS code?

An HMS code is the error message that Bambu Lab printers show on screen. You’ll find its meaning in the Bambu Lab, Creality, Elegoo and Anycubic error codes.

How can I tell if my PLA is damp?

Manufacturers mention small popping sounds as the plastic leaves the nozzle, a matte, uneven surface, and more stray threads than usual. Then dry the spool following the manufacturer’s instructions or with a filament dryer, and store it in a closed box.

Sources

  1. https://wiki.bambulab.com/en/filament
  2. https://www.creality.com/
  3. https://www.elegoo.com/

Sources checked on 30 October 2026. Printer prices shown are from official European stores in late October 2026 and may change. Technical figures come from manufacturer sheets and our calculations.

Written by Emmanuel Sauvage · Scan3D Lab

Was this page helpful?

A question about this machine or guide? Ask it here

We read every message and reply by email, usually within a few days.